Effect of Wood Self Factors on Bond Strength


Wood bonding technology plays an important role in the wood industry, and the bonding performance of wood bonding products is largely affected by the performance of the wood itself. The factors that affect the bonding performance of wood are both inherent in wood and produced in the process of wood processing. The former includes wood density, tree species, extract, pH, etc., and the latter includes wood moisture content, surface roughness, etc.
The strength of wood is usually proportional to its density, because the amount of wood cell wall material contained in the unit volume is the material basis for determining the strength of wood, and the strength of wood increases with the increase of wood density. For an ideal bonding system, bonding failure should occur in the xylem.

Many bonding tests of broad-leaved wood have proved that when wood is bonded with urea-formaldehyde resin adhesive, under the condition that the wood density is less than 0.8g/cm3, because the cohesive strength of urea-formaldehyde resin adhesive itself and the interfacial strength between urea-formaldehyde resin adhesive and wood are greater than the strength of wood itself, the bonding failure often occurs in the weakest link of the bonding system-wood. Therefore, the bonding strength is closely related to the strength of wood. Generally speaking, the bonding strength increases with the increase of wood density. In the case of wood density greater than 0.8g/cm3, due to the cohesive strength of the urea-formaldehyde resin adhesive itself and the interface strength of the urea-formaldehyde resin adhesive and wood is less than the strength of the wood itself, the bonding failure does not occur in the wood part, but occurs in the adhesive layer or interface, therefore, in this case, the bonding strength is almost independent of the wood density. When using resorcinol formaldehyde resin adhesive to bond all needles and broadleaved wood, the adhesive strength of wood glued products bonded with resorcinol formaldehyde resin adhesive increases with the increase of the density of the bonded wood due to the large cohesive force of the resorcinol formaldehyde resin adhesive.

Although the bonding strength of the high-density wood-bonded product is high, the stress generated due to the change of the moisture content is also large. In the case of adhesive determination, the bonding durability of wood with high density is often worse than that of wood with low density. For example, with water-based polymer isocyanate adhesive manufacturing of oak wood, although the compression shear strength is relatively large, but when the use of environmental humidity changes, more prone to cracking of the adhesive layer. In addition, the density of wood bonding, in order to achieve the ideal bonding effect, the requirements of the adhesive itself should also be very high, so as to give full play to the strength of the wood itself. For particularly high-density wood, such as ebony, wood bean, etc., the adhesive is not easy to be absorbed, so that the adhesive drying speed is very slow, the bonding strength is low. Therefore, for wood with a particularly high density, in order to make the adhesive penetrate into the cells, it is required to sand and glue on both sides, and to wait for sufficient time for the adhesive to penetrate before applying pressure. Sometimes, it is necessary to use polyurethane adhesives, because the bonding of this type of adhesive does not depend on its penetration, mainly chemical bonding.
2. Wood fiber direction and cutting plane direction Wood is an anisotropic material. The directions of wood fibers in the bonding system can be perpendicular to each other, parallel to each other, or at an angle to each other. When two pieces of wood are bonded in the same fiber direction, the bonding strength is the largest, such products as laminated wood and laminated veneer lumber (LVL), etc.; commonly used wood products that are bonded vertically to each other in the fiber direction include plywood, three-layer solid wood composite flooring, etc. With the increase of the fiber angle between the two pieces of bonded wood, the bonding strength of the bonding material gradually decreased. When the fiber direction is perpendicular to each other, the bonding strength is the lowest, and compared with the wood fiber parallel to each other, the bonding strength is only 1/4 to 1/3 of the fiber parallel to each other. The sectioning direction of the bonding surface also affects the bonding strength. Martin et al. studied the influence of wood fiber direction on the penetration of liquid adhesive into the wood surface, which showed that when the adhesive was applied to the wood end face, since the wood ducts and tracheids on the end cut face were open, the adhesive would penetrate into the cell cavity of these cells in large quantities, which would easily lead to the lack of adhesive on the end face, resulting in a decrease in the bonding strength of the wood. Therefore, under the same bonding conditions, the bonding strength of the end face and the end face is lower than that of the diameter face and the diameter face, the chord face and the chord face.
In actual work, if it is necessary to use the end cut surface bonding, in order to prevent its lack of glue, the viscosity and solid content of the adhesive must be increased; The use of two glue, or in the substrate on both sides of the glue, or increase the thickness of the glue layer; Use moderate pressure and prevent glue extrusion. For example, when the wood is longitudinally connected by butt joint, the above measures can be taken to avoid the lack of glue at its end. Under the condition that the fibers are bonded parallel to each other, the bonding surface can also be divided into radial and chord sections. In some cases, there is also a difference in the bond strength between the diameter section and the chord section. When the cohesive force of the adhesive and the interfacial strength between the adhesive and the wood are greater than the strength of the wood itself, the wood is prone to failure. If there is a difference in the strength of the wood's own chord and diameter sections, there is also a difference in the bond strength between the chord and chord sections and the diameter and diameter sections.

For example, the radial shear strength of larch wood is greater than its chordwise shear strength. When the larch plate is bonded with water-based polymer isocyanate adhesive, the normal compressive shear strength of the larch diameter cutting plate is higher than that of its string cutting plate. However, the wood breakage rate of larch string cutting board and string cutting board glued products is relatively high, which is basically wood damage, and most of the wood damage occurs at the junction or wheel boundary of the sudden change of wood in the morning and evening (therefore, when using API adhesive to produce larch glulam, diameter cutting board should be used for bonding as much as possible. 3 Wood moisture content Wood moisture content has a great influence on bonding performance. When the moisture content of the wood is high, the adhesive coated on the bonding surface is diluted, its viscosity decreases, and it is excessively soaked into the wood tissue, causing the lack of glue, resulting in a decrease in the bonding strength. Wood is dried at high temperature for a long time, and its moisture content is too low, which will weaken the wetting effect of the adhesive and reduce the bonding strength. Usually wood moisture content of 5% to 16% when the bonding strength is higher.
In addition, the wood has dry shrinkage and wet properties, if the wood moisture content is too low, its products will be affected with moisture and expansion; moisture content is too high, and will be desorbed dry shrinkage. Generally speaking, the adhesive itself cannot resist the very high stress caused by the expansion and drying of wood, which is a major cause of cracks and deformation in wood products. This happens when furniture is produced and used. The equilibrium moisture content of the wood where the furniture is produced and where it is used is often inconsistent, which requires the moisture content of the wood used in the production of furniture to be as close as possible to the humidity of the environment. For example, furniture purchased in Guangzhou is easy to crack when transported to Xinjiang, which requires that the moisture content of wood used by furniture manufacturers should be close to the equilibrium moisture content of wood in the location of the customer who purchased the furniture. Considering the lag of wood drying moisture absorption, in general, the final moisture content of wood drying and the equilibrium moisture content of wood in the use area are about 2%.
4 The shrinkage expansion rate of wood due to the natural shrinkage of the adhesive during curing and the difference in the properties of the adhesive and the wood, resulting in the existence of internal stress in the bonding joint, the concentration of internal stress will reduce the bonding strength. In order to reduce the stress caused by heat alternation or high temperature curing and cooling, the thermal expansion coefficient of the adhesive and the wood should be as close as possible.

There are two main ways to reduce internal stress: one is to add fillers, and the other is to select adhesives with good elasticity. When bonding wood with other materials, if the shrinkage rate difference between the materials is too large, measures should be taken in advance to reduce the dimensional change of the wood, or use an adhesive with excellent elasticity for bonding. For example, when metal-wood bonding, the hydroxyl component in wood causes wood dry shrinkage and swelling through moisture absorption or desorption, which is the main reason for the poor dimensional stability of wood. The dimensional stability of wood can be improved and the strength of modified wood can be improved by blocking the hydroxyl groups of wood and forming chemical crosslinking between hydroxyl groups. Therefore, the wood is treated with phenolic resin in advance, and the metal is bonded after its size is fixed, which can reduce the stress caused by the difference in shrinkage between the two. Another example, the use of veneer or plywood and foam board composite made of partition board, the first veneer or plywood fixed size, and then with the foam board composite effect will be better.
5. Surface processing method The bonding plane of the wood must be smooth and straight. If it is uneven (bending or warping), the two planes cannot be in close contact, which will affect the strength and quality of the bonding. Therefore, the wood is mechanically processed before the bonding operation, which may cause mechanical damage to the wood cells, and the degree of damage varies with the type and degree of machining. During planing processing, the surface wood tissue is less damaged, the inner cavity of wood cells is open, and the adhesive is easy to form effective glue nails after immersion. In order to reduce the damage to the wood tissue, the planer must be kept sharp, otherwise the damage to the wood tissue will be more serious. A.P.Singh found that the surface of radiata pine (P.radiate) wood planed with a sharp planer has a normal shape, except for a slight damage to the tracheids adjacent to the glue layer. The glue layer between the wood surfaces is thin and has a normal width (see Figure 3). In contrast, the surface of radiata pine wood planed with a blunt planer was severely damaged by axial tracheids and rays. Because the planer knife is blunt, the cells are severely crushed, especially the crushing of the cells next to the adhesive layer is likely to occlude the cell cavity and prevent the adhesive from penetrating into the cells, resulting in a thicker and uneven thickness of the adhesive layer. The fine planing of the wood surface helps to ensure the uniformity of the adhesive layer on the surface of the adhesive. The planing of the surface of the wood can expose the S2 layer of the cell wall with strong polarity, which is very beneficial to bonding. Although sanding will make the surface of the wood very smooth, the inner cavity of the wood tissue is damaged more, at the same time, some large surfaces are very smooth, and the cavity is easy to be blocked by sanding powder. Therefore, the bonding strength is lower than that of planing.
6 wood surface characteristics due to the wood is porous material, when two pieces of wood surface bonding, the actual only a small part of the apparent area of contact, and the area with the wood structure, surface roughness and the applied pressure and other factors vary. In other words, even if the pressure applied during bonding is not very large, the bonding material may withstand a relatively high pressure or even be crushed in a small part of the contact area. Generally speaking, a certain roughness of the surface, its concave and convex, pores and grooves are conducive to the penetration of the adhesive, can produce a mechanical bonding effect. However, when the roughness is too large and the concave holes and grooves on the surface are too deep, the residual air or adsorbed moisture will hinder the penetration of the adhesive and is not conducive to bonding.
7 wood surface passivation to keep the wood surface clean, to prevent pollution is the basic condition of its good bonding. In addition to air pollution (such as dust particle pollution in the air), the wood surface is also prone to a "self-pollution" over time, which changes the surface properties of the wood and affects the bonding properties of the wood.
 
Wood in the cutting process within a few hours, the oleophilic, low molecular weight substances will move to its surface to form a low surface energy of the "weak interface layer" wood surface experienced this change is often referred to as "surface passivation", the rate and degree of passivation according to wood species and storage temperature varies. The lipophilic substances in wood are mainly composed of resin, fatty acid and its esters, paraffin and terpene compounds. Acidic and neutral adhesives cannot easily penetrate this lipophilic layer, but alkaline adhesives can saponify fatty acids to some extent, so that the lipophilic layer disappears, so that the adhesive can penetrate well into the wood. R.M. Russbaum found that the surface wettability of European spruce (Picea abies) wood decreased significantly after 3 days of cutting. Therefore, he pointed out that the maximum storage time for European spruce wood used for coating and bonding to avoid surface passivation is 3 days, and it should be used within 2 to 3 days after processing to avoid natural surface passivation and affect its bonding strength.

In the production of wood glued products, it should be emphasized that the wood should be planed or sanded within 24h after the completion of the bonding operation. For example, in the production of laminated timber, the wood shall be bonded and pressurized as soon as possible after planing or milling the finger tenon, and the bonding and pressurizing shall not exceed 24h from planing or milling the finger tenon. In order to eliminate the "self-pollution" of the wood surface and the influence of the surrounding environmental pollution on the wetting of the wood surface, the wood surface should be effectively pretreated before bonding. Wood surface treatment can be used mechanical and chemical methods: cleaning with solvent, cleaning the bonding surface of the wood, so that the bonding surface as large as possible; mechanical methods (planing or sanding) to remove surface contaminants, while improving surface roughness to increase the bonding surface area.
8 Extracts of wood Extracts of wood have a certain influence on the wetting, penetration and curing process of the adhesive. In general, the extraction of more components of the wood, it is difficult to be fully wet by the adhesive, and the bonding strength is poor. When wood that is difficult to glue, such as Dipterocaceae wood, is boiled in hot water at 100 ℃ for 24 hours, a water-soluble gum composition accounting for 5% ~ 8% of the weight of the wood will be proposed. However, for Liu 'an and other woods with good gluing performance, when boiled under the same conditions, the extracted components only account for 0.1-0.2. It is also possible to add a surfactant to hot water or alkaline water for cooking, but this requires a lot of cost, so there is a certain difficulty in practical application.
For larch, Pinus massoniana and other resin-containing wood, it is first dried at high temperature to make the resin seep from the wood, then the surface is cleaned with a solvent to remove the resin, and then the surface is planed. Wood surface treatment immediately after the completion of the bonding, to prevent re-overflow resin. Phenolic adhesives are recommended for bonding.
9 the pH value of wood affects the curing time of the adhesive. For example, poplar, especially the pH value is alkaline, can prolong the curing time of urea formaldehyde resin adhesive. Because the urea-formaldehyde resin is cured under acidic conditions, and the alkaline poplar wood will reduce the acidity of the adhesive. Adding more curing agent and adjusting the pH value to 4.0~5.0 is the simplest way to solve the effect of poplar alkalinity on the curing time of urea-formaldehyde resin. In actual production, NH4C1 or mixed curing agent can be used according to the actual situation, such as adding some acid to the ammonium salt. Acidic wood, such as oak (pH 3.5), high acidity will hinder the gel time of some adhesives cured under alkaline conditions. On the contrary, it is beneficial to shorten the curing time of urea-formaldehyde resin adhesives.