Some precautions for using glue when the seasonal environment changes
The good composite effect of two-component polyurethane adhesive is related to many conditions, and the change of working environment is also an important factor. That is to say, with the change of seasonal climate, in order to obtain the ideal composite effect, it is necessary to make some fine adjustments to the glue use process.
To put it simply, the seasonal climate change that affects the compound is the change of the two major indicators of environmental humidity and temperature: specifically, in spring and summer, especially during the plum rains season, the relative humidity of the air is relatively high and can even reach saturation, while in autumn and winter, the air is dry and the humidity is low; in terms of temperature, summer is much higher than winter, the maximum difference between the two can be nearly 30~40 ℃ (here is to compare the southern area without indoor heating as an example). If these differences are not paid attention to, the following problems are likely to occur during compounding: when the air is humid, the glue is often not cured completely, that is, it is not dry and has large residual viscosity. In serious cases, wire drawing can even be observed during peeling of the composite film, especially when the film itself has large moisture absorption, such as when nylon film is used for compounding, this phenomenon is more likely to occur. Secondly, moist air will condense on the gluing anilox roller, thus bringing water into the glue basin. With the passage of time, the glue gradually changes from transparent to chaotic and whitish, and even loses its bonding effect. Damp, heat and high temperature also make it difficult to preserve glue. If the prepared working glue solution is not used up on the same day, it will often turn white and agglomerate to form gel (jelly gel-like) after being left overnight. In contrast, when it is cold in winter, the previously unused working glue solution still maintains good transparent fluidity overnight, and even can be directly used on the machine without being mixed into the newly prepared working glue solution in batches. On the other hand, in the winter when the temperature is low, the glue will become sticky and the leveling will decrease. When the laminating machine is running at high speed, a large number of bubbles are easy to accumulate on the glue surface and the edge of the gluing anilox roller in the glue basin, which may cause cavitation transfer, insufficient gluing amount and affect the compound fastness. At the same time, due to poor leveling dispersion performance, the appearance effect of the composite film will also deteriorate. For example, the flow pattern of glue is obvious, sometimes orange peel. When used for composite aluminum foil or aluminized film, if the printing surface has a large area of white ink or light ink, it is easier to form small white spots and spots. In addition, due to the low temperature in winter, the temperature of the curing room is very different from the external environment temperature. If the heat preservation measures are not in place, the heat loss rate is much faster than that in high temperature summer, which often makes the temperature in the curing room not reach the set temperature (generally 50 ℃). Therefore, the effect of curing is also affected to a certain extent. Under the same curing time, the compound fastness may be lower than that in summer.
To analyze the causes of the above phenomenon, it is necessary to understand the influence of moisture and temperature on the adhesive. First of all, for the two-component polyurethane adhesive, the water can react with the NCO group in the curing agent as the main agent, I .e. polyester/polyether polyol. It is estimated that 1g of water can consume 26~32g of curing agent. Of course, this is the pure reaction weight ratio. In practice, the water mixed into the working glue is competitive with the main agent when reacting with the curing agent. However, no matter how much water is involved in the reaction, it undoubtedly consumes the curing agent, making the amount of reaction with the main agent less than the original set of working ratio, thus causing incomplete curing and residual viscosity. The viscosity and reactivity of the adhesive are closely related to temperature. The viscosity value given by the adhesive manufacturer is measured by a rotational viscometer at a standard temperature of 25 ℃, which means that the temperature of the working environment can be more than 10 degrees higher in summer and more than 20 degrees lower in winter when it is cold. The viscosity of the glue is just the opposite of the temperature, that is, the same glue at high temperature shows a lower viscosity value, good flow dispersion performance, low temperature is high viscosity, poor flow. In addition, the crosslinking and curing reaction between the two components of the adhesive, the reaction speed is slow when the temperature is low, and the reaction speed is fast when the temperature is high, which is precisely why there is a curing room (accelerate the curing reaction speed and improve production efficiency).
In view of this situation, the following adjustments can be made according to environmental changes when using two-component polyurethane adhesive for compounding: if the air is humid and the temperature is too high, the dosage of curing agent should be appropriately increased by 10% ~ 20% to make up for the consumption of water; Dry cotton yarn or cloth is often used to absorb the condensed water droplets on the laminating machine to prevent them from falling into the glue basin. A small amount of solvent can be added to dilute the unused working glue, then sealed storage, if conditions permit, can be placed in a small freezer refrigerated storage, so that the effect is better, the next time again, in the case of closed thawing, and mixed with the newly equipped working glue. When the temperature is low in winter, the preparation of working glue can be appropriately added with more solvents to reduce the viscosity of the system, improve the leveling and dispersion, and also reduce the production of bubbles in the glue basin during work. However, the concentration of the working glue solution will be reduced. If the working concentration is not changed, a small amount of acetone can be used to replace part of ethyl acetate, that is, a mixed solvent of acetone and ethyl acetate is used as a diluent, and the ratio of the two can be 2:8 or 3:7. In addition, the temperature of the curing room can be set slightly higher in winter to ensure that the actual temperature can meet the requirements, so as not to affect the curing effect.
Previous Page